Still not perfect, but a much smoother first layer. In addition, slowing down the print speed of your first layer is often well worth the extra print time. I've found this to be especially true when using the PC+PBT filament for the base, screen back and hinge. My failure rate with that filament was around 50%, but when I slowed down the first layer print time to 40% speed, I haven't failed a print yet.
Thought maybe this could help someone else too! I print on a Prusa i3 mk2S.